Extrusion & Post 11 görüntüleme

Glass Fibre vacuum section material overflow

Sorun Belirtisi
Glass Fibre extrusion vacuum section material overflow, vent hole clogged
Neden Analizi
Glass Fibre melt viscosity low, overflows at vacuum section; vacuum section temperature too high, viscosity lower, aggravates overflow; vent hole design improper
Çözüm
1) Reduce vacuum section temperature 5-10°C to raise viscosity; 2) add baffle above vent hole to prevent overflow; 3) raise screw speed to accelerate conveying and reduce residence
Temel Çıkarım
Material overflow is caused by low melt viscosity; cooling and adding baffle are key
Glass Fibrevacuum section overflowmelt viscositycoolingvent baffle