Processing Machinery 3 görüntüleme

Glass Fibre internal unmelted particles

Sorun Belirtisi
Glass Fibre product interior shows unmelted transparent or translucent particles
Neden Analizi
Screw plasticizing capacity insufficient, temperature too low; feed amount too large, exceeding plasticizing capacity; Glass Fibre melting temperature too high
Çözüm
1) Raise processing temperature to ensure full melting; 2) reduce feed amount to match plasticizing capacity; 3) increase screw mixing section
Temel Çıkarım
Unmelted particles are caused by insufficient plasticizing; raising temperature and reducing feeding are key