Extrusion & Post 11 görüntüleme

MP extruded film poor thickness uniformity

Sorun Belirtisi
MP extruded film transverse thickness deviation ±15%, exceeding the ±5% industry standard
Neden Analizi
die flow channel design unreasonable causing uneven melt flow in the wide die; MP melt elasticity large, extrusion swell uneven; air ring cooling uneven
Çözüm
1) adopt a coat-hanger die design to ensure uniform transverse flow; 2) fine-adjust die gap ±0.02mm; 3) optimize air ring air volume and angle for uniform cooling; 4) add a small amount of low-elasticity resin to reduce swell difference
Temel Çıkarım
film thickness uniformity requires coordinated optimization from die design, gap adjustment and cooling
MP film thickness uniformity die design extrusion swell air ring cooling