MP Low Flexural Modulus
Sorun Belirtisi
Flexural modulus of MP products <20% of design value
Neden Analizi
MP is soft with low modulus; insufficient filler addition or poor interface failing to provide reinforcement; low crystallinity
Çözüm
1) Add 10-15wt% rigid filler to increase modulus; 2) Nucleating agent to increase crystallinity; 3) Select high-modulus grades
Temel Çıkarım
Low flexural modulus is caused by soft material and insufficient filler; adding rigid filler is key