Extrusion & Post 11 görüntüleme

MP Surface Snakeskin Pattern

Sorun Belirtisi
Snakeskin-like irregular texture on the surface of MP extruded products
Neden Analizi
Extrusion temperature too low with non-uniform melt elastic recovery; uneven die temperature distribution
Çözüm
1) Increase extrusion temperature to the processing temperature range; 2) Homogenize die temperature to ±2°C; 3) Reduce extrusion rate to reduce elastic recovery
Temel Çıkarım
Snakeskin pattern is caused by low-temperature extrusion and elastic recovery; increasing temperature and reducing speed are key
MPSnakeskin PatternExtrusion TemperatureElastic RecoveryDie Temperature Control