Extrusion & Post 11 görüntüleme

MP Internal Delamination Cracking

Sorun Belirtisi
Internal delamination of MP products cracking along the interface
Neden Analizi
Poor interfacial bonding between MP and incompatible fillers or blend components; cooling shrinkage differences causing interlayer stress
Çözüm
1) Use compatibilizer to improve interfacial bonding; 2) Uniform cooling to reduce interlayer stress; 3) Reduce the addition amount of incompatible components
Temel Çıkarım
Internal delamination is caused by poor interface and shrinkage differences; compatibilizer and uniform cooling are key