Problem of bubble of high-temperature resistant masterbatch in PET applications
Sorun Belirtisi
High-temperature resistant masterbatch shows bubble during high-temperature processing of PET.
Neden Analizi
Improper matching between carrier resin and matrix.
Çözüm
Solve by optimizing pigment/additive temperature resistance.
Temel Çıkarım
The key of high-temperature resistant masterbatch lies in carrier resin matching.