Problem of masterbatch agglomeration of high-temperature resistant masterbatch in PEEK applications

Sorun Belirtisi
High-temperature resistant masterbatch shows masterbatch agglomeration during high-temperature processing of PEEK.
Neden Analizi
Improper pigment temperature resistance of carrier resin.
Çözüm
Solve by adjusting the masterbatch concentration.
Temel Çıkarım
The key of high-temperature resistant masterbatch lies in carrier resin matching.