Control of strength abnormality in PEOX cast film water-soluble bags
Sorun Belirtisi
During PEOX cast film production of water-soluble bags, the problem of unstable strength occurs.
Neden Analizi
Mainly due to the processing temperature deviating from the window +70-90°C, moisture content >0.3% exceeding the standard, and shear heat accumulation.
Çözüm
Strictly control the temperature within the recommended range, fully dry the material to moisture content <0.1%, and reduce the screw speed.
Temel Çıkarım
PEOX processing requires precise control of the three elements of temperature, humidity, and residence time.