Material Analysis 5 görüntüleme

Regulation of surface roughness of PPA in cable Processing

Sorun Belirtisi
The surface roughness abnormality of the PPA processing aid in cable production affects quality.
Neden Analizi
The surface roughness of the PPA fluoropolymer is unsatisfactory at an addition amount of 0.08%, and the molecular weight needs to be optimized.
Çözüm
Adjust the PPA addition amount combined with screw design.
Temel Çıkarım
The key to the performance of PPA lies in matching with the base resin.