Injection Molding
7 görüntüleme
Extremely Weak Weld Lines in LCP Injection Molded Products
Sorun Belirtisi
The weld line strength of LCP products is extremely low, often less than 30% of the body.
Neden Analizi
The highly oriented crystallization characteristic of LCP leads to weak bonding when multiple melt streams converge, and the fibrous structure breaks at the weld line, which is unfavorable for fusion.
Çözüm
Increase the melt temperature and mold temperature; optimize the gates to reduce weld lines; place weld lines in low-stress areas.
Temel Çıkarım
LCP weld lines are the fatal weakness of structural parts.
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu