Injection Molding 7 görüntüleme

PPS '2079851475616104452 insufficient crystallization poor performance

Sorun Belirtisi
The mechanical and heat resistance properties of PPS products are not as expected.
Neden Analizi
PPS requires a high-temperature mold of 130-150°C to ensure full crystallization; when mold temperature <100°C, crystallization is incomplete, and HDT and strength decrease significantly.
Çözüm
Use oil temperature machine or electric heating mold, maintain mold temperature 140-150°C; ensure sufficient holding pressure and cooling time.
Temel Çıkarım
The excellent performance of PPS highly depends on sufficient crystallization.
PPScrystallizationmold temperatureHDToil temperature machine