Injection Molding 7 görüntüleme

POE '2079851475616104452 multi-cavity filling imbalance

Sorun Belirtisi
POE injection 8-cavity mold, cavity filling amount difference ±15%, some cavities short shot, some flash
Neden Analizi
Runner design unbalanced, runner length and resistance of each cavity inconsistent; gate sizes of each cavity inconsistent
Çözüm
1) Adopt balanced runner design to ensure equal length and equal resistance of runners to each cavity; 2) Gate sizes of each cavity precisely consistent ±0.01mm; 3) Reduce injection speed to reduce resistance difference influence; 4) Use mold flow analysis software to optimize runner design
Temel Çıkarım
Multi-cavity filling imbalance is caused by runner design; balanced runners and mold flow analysis are key
POE injectionmulti-cavity balancerunner designgate sizemold flow analysis