Extrusion & Post
5 görüntüleme
Poor leveling of powder coatings
Sorun Belirtisi
Electrostatic sprayed coatings have an orange peel appearance
Neden Analizi
The powder particle size is too coarse and the distribution is wide; the heating rate is slow
Çözüm
Control D50 at 30-50um, rapid temperature rise to 240-250C
Temel Çıkarım
Leveling directly affects the appearance quality of the coating
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu