Excessive Gel/Gel Particles in High-Density Polyethylene Extruded Products

Sorun Belirtisi
Transparent or translucent gel particles (gel particles) are visible in the extruded film or product, affecting the product appearance and transparency. Gel is resin particles that are not fully plasticized or cross-linked.
Neden Analizi
(1)The high-molecular-weight components in the raw material are not fully plasticized (2)The barrel temperature is low, and part of the resin is not completely melted (3)The screw mixing effect is insufficient (4)The raw material contains cross-linked or oxidized gel (5)The filter screen mesh count is not enough, and the gel is not intercepted
Çözüm
(1)Appropriately increase the barrel temperature to a higher value within the 180-260°C range (2)Optimize the screw design and add mixing elements (3)Increase the filter screen mesh count to 80-120 mesh (4)Select high-quality raw materials with low gel content (5)Check whether cross-linked materials are mixed into the regrind
Temel Çıkarım
Gel is caused by insufficient plasticization or raw material quality problems, and needs to be solved from temperature control, screw design, and raw material selection.
gelgel particleplasticizing temperaturescrew mixingfilter screen mesh count