Extrusion & Post
9 görüntüleme
Metallocene linear low density polyethylene cast film uneven thickness(Variant: Strengthened Measures)
Sorun Belirtisi
The transverse thickness deviation of the cast film is large, exceeding the tolerance range.
Uneven thickness affects film winding quality and subsequent processing, and affects service performance in precision films.In particular, extra attention is needed on top of the original basis, this problem is more prominent and requires key attention.
Neden Analizi
(1) The T-die lip gap is uneven\
(2) The die temperature distribution is uneven\
(3) The air knife airflow is uneven\
(4) The cooling roll temperature is uneven\
(5) Extrusion output fluctuates\
(6) On top of the original basis, extra attention is needed: process parameter fluctuations or equipment status changes aggravate this problem
Çözüm
(1) Adjust the T-die lip gap, use a feeler gauge to check uniformity\
(2) Check the die heater distribution, ensure transverse temperature difference does not exceed ±3°C (190-260°C range)\
(3) Check the air knife, ensure uniform air outlet, clean the air knife opening\
(4) Check the cooling roll temperature uniformity, temperature difference not exceeding ±2°C\
(5) Stabilize the extruder screw speed and temperature\
(6) And strengthen process monitoring; on top of the original basis, extra attention is needed, paying special attention to parameter stability
Temel Çıkarım
Cast film thickness unevenness is caused by die gap or temperature unevenness, and needs to be solved from mold precision and temperature uniformity.Targeted preventive measures need to be taken in different production scenarios.