Extrusion & Post 8 görüntüleme

Metallocene linear low density polyethylene film gel particles/gel granules(Variant: Strengthened Measures)

Sorun Belirtisi
Transparent or translucent granular gel particles are visible in the film, affecting film appearance and transparency. Gel particles are insufficiently plasticized resin or crosslinked gel, especially obvious in transparent films.In particular, extra attention is needed on top of the original basis, this problem is more prominent and requires key attention.
Neden Analizi
(1) The high molecular weight fraction in the raw material is not fully plasticized\ (2) Extrusion temperature too low\ (3) Insufficient screw mixing effect\ (4) The raw material contains crosslinked gel\ (5) The filter screen mesh count is insufficient\ (6) On top of the original basis, extra attention is needed: process parameter fluctuations or equipment status changes aggravate this problem
Çözüm
(1) Increase extrusion temperature to the higher value within the 190-260°C range\ (2) Optimize screw design, add mixing elements\ (3) Select high-quality raw material with low gel content\ (4) Increase the filter screen mesh count to 80-120 mesh\ (5) Regularly clean the screw and die to prevent carbide formation\ (6) And strengthen process monitoring; on top of the original basis, extra attention is needed, paying special attention to parameter stability
Temel Çıkarım
Gel particles are caused by insufficient plasticization or raw material quality problems, and need to be solved from temperature control and raw material quality.Targeted preventive measures need to be taken in different production scenarios.