Material Drying 15 görüntüleme

Bubbles/pores on the surface of random copolymer polypropylene extruded products

Sorun Belirtisi
Bubbles or pores appear on the extrudate surface or cross-section, and product density decreases. Bubbles not only affect appearance but also reduce product mechanical strength and pressure resistance; they are common in pipe and profile extrusion.
Neden Analizi
(1) Raw material moisture content exceeds the standard; moisture vaporizes at high temperature to produce bubbles (2) Poor screw venting; air is entrained in the melt (3) Barrel temperature is too high; material thermal degradation produces gas (4) Screw speed is too fast, and venting time is insufficient (5) Raw material has high content of low-molecular volatiles
Çözüm
(1) Fully dry the raw material; control random copolymer polypropylene moisture content below 0.02% (2) Check venting section design, and use a vented extruder if necessary (3) Appropriately lower barrel temperature to a reasonable value within the 190-260°C range (4) Reduce screw speed to increase material residence time in the venting section (5) Select raw material grades with low volatile content
Temel Çıkarım
Bubbles are caused by moisture vaporization or gas entrainment and need to be solved from raw '2079851475616104451 and the venting system.