Material Analysis 12 görüntüleme

Processing difficulty after adding thermally conductive fillers to PET

Sorun Belirtisi
After adding thermally conductive fillers (graphite, boron nitride) to PET, melt viscosity increases sharply, processing difficult, surface rough.
Neden Analizi
High filling amount (>30%) causes sharp fluidity decline, poor filler-matrix compatibility produces interfacial friction, uneven filler dispersion.
Çözüm
Use coupling agents to improve the interface; optimize screw configuration to improve dispersion; appropriately increase processing temperature; control filling amount ≤50%.
Temel Çıkarım
PET thermally conductive composite processability depends on filler selection and interface treatment.