Material Drying 5 görüntüleme

Large amount of smoke during PET '2079851475616104452

Sorun Belirtisi
A large amount of smoke and white fumes is produced during PET '2079851475616104452, the working environment deteriorates, and products have an odor.
Neden Analizi
Insufficient '2079851475616104451 with high moisture content vaporizing at high temperature; excessive processing temperature volatilizes low-molecular substances; oligomer content is high.
Çözüm
Ensure full drying (moisture ≤0.003%); reduce processing temperature; select low-oligomer raw materials; install a ventilation system.
Temel Çıkarım
PET '2079851475616104452 smoke mainly originates from moisture and low-molecular volatiles.
PETsmokemoistureoligomersventilation