Injection Molding 12 görüntüleme

Poor hot runner balance in PET '2079851475616104452

Sorun Belirtisi
The output of each nozzle of the PET hot runner system is uneven, and product weights of multi-cavity molds differ greatly.
Neden Analizi
The flow paths of each hot runner are unequal with different flow resistances; heating temperatures of each nozzle are uneven; rheological balance calculation was not performed.
Çözüm
Adopt natural balance or rheological balance design; use temperature-adjustable nozzles; optimize runners with mold flow analysis; regularly clean the hot runner.
Temel Çıkarım
PET hot runner balance is a core requirement of multi-cavity precision '2079851475616104452.
PEThot runnerbalancemulti-cavityflow resistance