Extrusion & Post 4 görüntüleme

Longitudinal streaks on PET extruded sheet

Sorun Belirtisi
Continuous or intermittent streaks along the extrusion direction appear on the PET sheet surface, with uneven gloss.
Neden Analizi
The die lip has scratches or material buildup; the three-roll surface is damaged or contaminated; the melt is mixed with impurities or degradation products.
Çözüm
Clean and polish the die lip; clean and repair the three-roll surface; check raw material cleanliness and clean dead zones of the extrusion system.
Temel Çıkarım
PET sheet surface streaks are mostly caused by mechanical damage or contamination; regular maintenance is the key to prevention.