PETG UV-curable coating insufficient adhesion

Sorun Belirtisi
After UV coating curing, the adhesion test is unqualified and the coating peels off.
Neden Analizi
PETG has low surface energy and poor coating wetting, the surface has contamination or an oxide layer, and the UV formulation is improper.
Çözüm
Surface corona or plasma pretreatment; optimize the UV formulation by adding adhesion promoters; increase UV curing energy.
Temel Çıkarım
PETG UV coating adhesion depends on surface treatment and formulation optimization.