Material Analysis 12 görüntüleme

Improvement of PLA modified heat distortion temperature

Sorun Belirtisi
The heat distortion temperature of PLA is low and needs to be raised to above 80-100°C.
Neden Analizi
PLA crystallization is insufficient or the matrix itself HDT (amorphous) is only 55-65°C.
Çözüm
Promote crystallization (nucleating agent + heat treatment) or alloy with high heat-resistant bioplastics.
Temel Çıkarım
PLA heat-resistant modification is the prerequisite for its high-end applications.