Molding Process
5 görüntüleme
Insufficient transparency of PLA products
Sorun Belirtisi
PLA products have poor transparency and large haze.
Neden Analizi
The PLA crystallinity is high (>20%) or the cooling conditions promote crystallization, causing the transparency to decrease; impurities are present.
Çözüm
Use amorphous PLA grades; rapidly cool to suppress crystallization; keep the raw material pure.
Temel Çıkarım
PLA transparency is negatively correlated with crystallinity.