Sorun Belirtisi
Products crack when contacting specific chemical media while simultaneously bearing stress.
Neden Analizi
(1) Residual stress exists in the product, accelerated cracking under chemical media action
(2) Contact with incompatible chemical media (solvents, oils, etc.)
(3) Uneven product wall thickness, stress concentration areas easily crack
(4) Low material molecular weight, poor environmental stress cracking resistance
(5) High use environment temperature accelerates cracking
Çözüm
(1) Reduce product residual stress (annealing treatment)
(2) Avoid contact with incompatible chemical media
(3) Optimize product design, uniform wall thickness, reduce stress concentration
(4) Select high molecular weight grades
(5) Reduce use environment temperature
Temel Çıkarım
Environmental stress cracking is the result of the combined action of stress and chemical media.