Yaygın plastik malzeme zorluklarına pratik yanıtlar

1506 soru
Q
Tiger Skin Pattern on CMC Surface
A
Tiger skin pattern is caused by unstable injection front; multi-stage injection and high mold temperature are the key
Injection Molding CMCtiger skin patterninjection speedmulti-stage injectionmold temperature control
Q
Obvious Surface Color Difference of CMC
A
Color difference is caused by uneven dispersion and orientation; masterbatch method and stable processing are the key
Injection Molding CMCcolor differencecolor masterbatch dispersionpigment orientationtemperature stability
Q
Orange Peel Texture on CMC Surface
A
Orange peel is caused by rapid cooling and solidification; increasing mold temperature and holding pressure are the key
Injection Molding CMCorange peelmold temperatureholding pressuresurface solidification
Q
Severe Internal Stress Concentration of CMC
A
Internal stress is caused by fast injection and uneven cooling; speed reduction, uniform cooling and annealing are the key
Injection Molding CMCinternal stressorientation stressannealing treatmentuniform cooling
Q
Unstable Weight of CMC Injection Molded Products
A
Product weight stability depends on injection amount accuracy and holding consistency
Injection Molding CMC injectionweight fluctuationinjection amountholding consistencyV/P switchover
Q
Cold Slug Marks in CMC '2079851475616104452
A
Cold slug marks are caused by solidified residual material in the nozzle; increasing nozzle temperature and cold slug well design are the key
Injection Molding CMC injectioncold slug marknozzle temperaturecold slug wellinjection pressure
Q
Flow Marks in CMC '2079851475616104452
A
Flow marks are caused by unstable injection front and rapid cooling; multi-stage injection and high mold temperature are the key
Injection Molding CMC injectionflow markinjection speedmold temperaturegate area
Q
Sink Marks in CMC '2079851475616104452
A
Sink marks are caused by insufficient holding and wall thickness differences; high-pressure holding and multiple gates are core countermeasures
Injection Molding CMC injectionsink markholding pressurewall thickness differencegate design
Q
Unbalanced Multi-Cavity Filling in CMC '2079851475616104452
A
Unbalanced multi-cavity filling is caused by runner design; balanced runners and mold flow analysis are the key
Injection Molding CMC injectionmulti-cavity balancerunner designgate sizemold flow analysis
Q
Ejector Pin Whitening on CMC Injection Molded Products