Menü
Malzemeler Makineler
İçgörüler
Makaleler Videolar Sorun ve Çözüm
About
Chembull Hakkında Medya Ortakları
Bize Ulaşın
Dil
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어

Sorun ve Çözüm

Yaygın plastik malzeme zorluklarına pratik yanıtlar

1506 soru
Q
PI compression molding and sintering product cracks
A
The heating and cooling control of PI sintering is the key to preventing cracking
Molds & Tooling compression molding and sinteringcrackspreformingheating ratecooling rate
Q
Product stress cracking
A
The stress cracking problem of PES can be solved by annealing and optimizing the design
Molds & Tooling stress crackingannealingmold temperaturesharp cornersdesign optimization
Q
Insufficient mold filling flow length
A
PES requires higher processing temperature and mold temperature to assist filling
Molds & Tooling mold fillingmelt temperaturemold temperaturemelt viscosityflow window
Q
PEI processing comprehensive problem - high-temperature mold
A
The processing quality management of PEI materials requires comprehensive attention to multiple dimensions such as high-temperature mold
Molds & Tooling PEIhigh-temperature moldprocessing qualityprocess optimizationequipment management
Q
Multi-gate product low weld line strength
A
The rigid molecular chain characteristics of PEI make weld lines particularly weak areas
Molds & Tooling weld linenumber of gatesmelt temperaturemolecular diffusionsequential valve
Q
Product dimensional accuracy difficult to control
A
The dimensional accuracy of PEI products is highly dependent on the stability of process parameters
Molds & Tooling dimensional accuracyshrinkage ratemold temperatureholding pressuretolerance control
Q
Pitting on the mold cavity
A
PEI processing has a certain chemical corrosiveness on molds, requiring corrosion-resistant mold materials
Molds & Tooling mold corrosionpittingS136PVD coatingstainless steel
Q
Product stress cracking
A
Annealing is an effective method to eliminate internal stress and prevent cracking in PEI products
Molds & Tooling stress crackingannealingmold temperaturestress concentrationsharp corners
Q
High-viscosity melt mold filling difficulty
A
Within the degradation and safety range, the PEI processing temperature should be increased as much as possible to improve flowability
Molds & Tooling filling difficultymelt viscosityMFRmelt temperaturemold temperature
Q
PEEK processing comprehensive problem - mold temperature
A
The processing quality management of PEEK materials requires comprehensive attention to multiple dimensions such as mold temperature
Molds & Tooling PEEKmold temperatureprocessing qualityprocess optimizationequipment management
Önceki 1 2 3 4 ... 151 Sonraki