Q
HDPE film poor opening
A
Opening is controlled by three controls: additives + tension + temperature.
Extrusion & Post HDPE; film; opening; blocking; slip agent
Q
HDPE blown film thickness deviation
A
Transverse thickness goes back to the die lip and air ring.
Extrusion & Post HDPE; blown film; thickness deviation; die lip; air ring
Q
HDPE blown film bubble instability
A
Stable bubble = stable extrusion + uniform air ring + quiet environment.
Extrusion & Post HDPE; blown film; bubble instability; air ring; extrusion fluctuation
Q
HDPE film gel (fisheye)
A
Plasticization of high molecular weight material is the foundation of gel prevention and control.
Extrusion & Post HDPE; blown film; gel; fisheye; plasticization
Q
HDPE extrusion screw slipping
A
For discharge pulsation, first check the feed section temperature and feeding.
Extrusion & Post HDPE; screw slipping; feed section; bridging; plasticization fluctuation
Q
HDPE pipe outer surface roughness
A
Surface roughness: check temperature, raw material, and cleanliness.
Extrusion & Post HDPE; pipe; surface roughness; temperature; regrind
Q
HDPE pipe ovality out of tolerance
A
Ovality = a synchronization problem of sizing + cooling + haul-off.
Extrusion & Post HDPE; pipe; ovality; vacuum sizing; haul-off