Extrusion & Post 5 görüntüleme

EVA film printing adhesion

Sorun Belirtisi
Insufficient printing adhesion.
Neden Analizi
The match between EVA surface polarity and ink needs verification; improper surface treatment affects adhesion.; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based on experience alone
Çözüm
①Corona treatment to increase surface energy; ②select matching ink; ③test the dyne value before printing; ④conduct adhesion tests.; after adjustment, take consecutive samples to verify the effect, and resume mass production only after confirming stability
Temel Çıkarım
Pre-treatment before EVA printing is indispensable; the dyne value is the release basis.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
EVA; film; printing; adhesion; corona; dyne value