Extrusion & Post
2 Aufrufe
EVA film printing adhesion
Problembeschreibung
Insufficient printing adhesion.
Ursachenanalyse
The match between EVA surface polarity and ink needs verification; improper surface treatment affects adhesion.; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based on experience alone
Lösung
①Corona treatment to increase surface energy; ②select matching ink; ③test the dyne value before printing; ④conduct adhesion tests.; after adjustment, take consecutive samples to verify the effect, and resume mass production only after confirming stability
Wichtigste Erkenntnis
Pre-treatment before EVA printing is indispensable; the dyne value is the release basis.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
War das hilfreich?
0 Personen fanden dies hilfreich
Vielen Dank für Ihr Feedback!