Yaygın plastik malzeme zorluklarına pratik yanıtlar

11636 soru
Q
POM '2079851475616104452 cycle too long
A
Cycle = cooling efficiency.
Injection Molding POM;cycle;cooling;water lines
Q
POM hot runner problem
A
Hot runner = a test of temperature control precision.
Molds & Tooling POM;hot runner;decomposition;temperature control
Q
POM product corner breakage
A
Corner breakage = sharp corners.
Molds & Tooling POM;corner breakage;sharp corners;ejection
Q
POM product flow marks
A
Flow marks = melt front.
Molds & Tooling POM;flow marks;mold temperature;speed
Q
POM injection molded product short fill—venting type
A
Fixed-point short fill = venting.
Injection Molding POM;short fill;venting;short shot method
Q
POM product static dust attraction
A
Static electricity = a common problem of insulating materials.
Molding Process POM;static electricity;dust attraction;antistatic
Q
POM product yellowing
A
Yellowing = precursor of decomposition.
Material Analysis POM;yellowing;decomposition;temperature
Q
POM injection molded product delamination
A
Delamination = contamination.
Extrusion & Post POM;delamination;contamination;release agent
Q
POM product dimensional instability
A
Dimension = crystallinity stability.
Molds & Tooling POM;dimension;crystallinity;mold temperature