Processing Machinery 6 مشاهدة

ABAK high damping low gloss

ظاهرة المشكلة
ABAK high damping low gloss grade; special needs for noise reduction and appearance.
تحليل الأسباب
ABAK high damping low gloss alloy; compounding of two ABS particle sizes; polyolefin elastomer; high damping coefficient; noise reduction effect; ultra-low gloss.;during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
الحل
①Special grade selection; ②formula compounding; ③performance testing; ④application matching; ⑤process stability.;after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
الخلاصة الأساسية
ABAK high damping low gloss is a differentiated grade; compounding technology is the core; testing verifies special performance.;after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
ABAK;high damping;low gloss;noise reduction;compounding;elastomer