Molding Process 6 مشاهدة

ABS vent depth

ظاهرة المشكلة
[Problem phenomenon] ABS vent too shallow causes trapped gas burnt, too deep causes flash
تحليل الأسباب
Vent depth 0.025-0.05mm: too shallow and gas cannot escape causing trapped gas burnt, too deep and melt overflows in causing flash; ABS fluidity determines this window
الحل
Vent depth precision machined according to 0.025-0.05mm; check vent first in trapped gas areas; check whether vent is too deep for flash; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
الخلاصة الأساسية
ABS vent 0.025-0.05mm, shallow traps gas and deep causes flash; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems
vent depth trapped gas flash