Injection Molding 7 مشاهدة

ABS flow mark

ظاهرة المشكلة
[Problem Phenomenon] ABS surface corrugated flow marks
تحليل الأسباب
Front cold film rupture; mold temperature low and injection speed slow; during on-site troubleshooting, verify item by item according to this mechanism, avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry materials and should be confirmed first during troubleshooting
الحل
Raise mold temperature and melt temperature; multi-stage injection optimization; enlarge runner and gate; after adjustment, continuously sample to verify the effect, resume mass production only after confirming stability; change only one variable each time and record parameter changes to facilitate locating effective measures
الخلاصة الأساسية
For ABS flow marks raise temperature and stabilize speed; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems later
flow mark mold temperature injection speed multi-stage

هل كان هذا مفيدًا؟

0 شخص وجدوا هذا مفيدًا

ChemAI