Production & Quality 6 مشاهدة

ASA Vicat softening 101°C

ظاهرة المشكلة
ASA Vicat softening point average 101°C, heat resistance boundary.
تحليل الأسباب
ASA Vicat softening point average 101°C range 85-133°C; heat deflection temperature; continuous use temperature; application boundary; heat resistance management; grade differences.
الحل
①Vicat 101°C reference; ②heat deflection evaluation; ③continuous use temperature; ④application boundary; ⑤grade selection.; After adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
الخلاصة الأساسية
ASA 101°C Vicat is a heat resistance reference; boundary management ensures application; grade matches demand.; After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
ASA;Vicat softening;101°C;heat deflection;continuous;boundary