Processing Machinery 6 مشاهدة

ASA Low-Temperature Application Scenarios

ظاهرة المشكلة
【Problem Phenomenon】Outdoor parts in cold regions crack brittle in winter, material low-temperature toughness insufficient
تحليل الأسباب
ASA glass transition temperature is about 97-100℃, low-temperature toughness is better than most styrenics; outdoor parts in cold regions still need low-temperature impact verification; during on-site troubleshooting, verify item by item according to this mechanism, avoid blindly adjusting the machine based only on experience
الحل
Cold region parts choose ASA and do -30℃ impact verification; structure rounded; toughened grades cover extreme cold; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
الخلاصة الأساسية
ASA low-temperature toughness is above average, cold region parts can be used with confidence after verification; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems
low temperature cold region impact toughening

هل كان هذا مفيدًا؟

0 شخص وجدوا هذا مفيدًا