COC Improper Mold Temperature Setting Poor Surface

ظاهرة المشكلة
COC optical parts have poor surface replicability, obvious flow marks, uneven gloss, increasing injection speed gives limited improvement, surface quality never reaches optical grade.
تحليل الأسباب
COC is an amorphous material, mold wall temperature has great influence on surface replication; when mold temperature is too low the melt surface layer is quenched and cannot replicate the cavity mirror; high surface requirement parts need high mold temperature close to Tg.
الحل
①Raise mold temperature to the range about 10℃ below Tg and match with high injection speed; ②the higher the surface requirement the higher the mold temperature; ③verify mold heating capacity reaches 95~130℃ range; ④cavity mirror polishing matched.
الخلاصة الأساسية
The core lever of COC surface quality is mold temperature; high mold temperature process close to Tg is standard for optical parts; mold temperature controller selection must cover the high-temperature section with precise control.
COC; mold temperature; surface; optical; Tg; flow mark