Extrusion & Post 6 مشاهدة

LLDPE blown film transverse tear

ظاهرة المشكلة
Film transverse tear strength is poor, and bag sides crack easily after bag making
تحليل الأسباب
Insufficient blow-up ratio leaves transverse molecular chains not fully extended; LLDPE's extensional softness makes transverse orientation harder; biaxial mechanical properties are unbalanced; when troubleshooting on site, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience
الحل
①Increase blow-up ratio to 2-4 times to balance biaxial properties; ②dual-lip air ring enhances transverse cooling and setting; ③verify tear strength by application; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
الخلاصة الأساسية
LLDPE transverse tear is opened up by the blow-up ratio; the 2-4 times range plus dual-lip air ring setting is the standard combination; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
LLDPE;transverse tear;blow-up ratio;dual-lip air ring