PA6 Rotational Molding
ظاهرة المشكلة
Rotomolded PA6 products have uneven wall thickness, internal bubbles, and insufficient strength at corners
تحليل الأسباب
Rotational molding relies on powder melting and self-leveling; PA6 has a high melting point and low melt strength, with insufficient accumulation at corners; moisture in the powder vaporizes during long-time heating, forming internal bubbles
الحل
①Strictly control the moisture content of rotomolding-specific powder; ②enlarge the fillets at mold corners to improve material flow; ③optimize the heating curve according to the melting point peak; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
الخلاصة الأساسية
PA6 rotational molding is sensitive to powder state and mold geometry; fillet design and powder drying are the keys to eliminating corner defects and internal bubbles; after confirming effectiveness, fix the parameters and practices into the work instructions to prevent recurrence
هل كان هذا مفيدًا؟
0 شخص وجدوا هذا مفيدًا
شكرًا لك على ملاحظاتك!