Injection Molding 8 مشاهدة

PA6 Injection Speed Strategy

ظاهرة المشكلة
Jetting marks appear on the surface, or incomplete filling appears after reducing speed for surface quality
تحليل الأسباب
PA6 usually requires filling as fast as possible to prevent solidification; but high speed in glass fiber reinforced grades aggravates floating fibers and jetting, forming a contradiction between surface quality and filling completeness
الحل
①Inject neat PA6 as fast as possible; ②Appropriately reduce speed for reinforced grades in exchange for surface quality; ③Use temperature to compensate for the filling loss caused by speed reduction; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
الخلاصة الأساسية
PA6 injection speed strategy must be set separately by grade; neat material seeks speed, reinforced material seeks stability, and temperature is the regulating valve between the two; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
PA6; injection speed; jetting mark; reinforced grade; surface quality