Extrusion & Post 6 مشاهدة

PC Extruded Sheet Uneven Thickness

ظاهرة المشكلة
PC extruded sheet/plate has large transverse thickness deviation, optical plates are unqualified.
تحليل الأسباب
Improper die lip gap adjustment, uneven melt temperature, and haul-off speed fluctuations all cause thickness deviation; uneven die head thermal expansion and local material accumulation also make the discharge uneven.
الحل
①Calibrate the die lip bolts and use closed-loop adjustment with a thickness gauge; ②Stabilize the melt temperature and the temperatures of each die head zone; ③Stabilize the haul-off speed, synchronized with extrusion; ④Clean the die head regularly; ⑤Check heating uniformity.
الخلاصة الأساسية
PC sheet thickness relies on the three-in-one stability of 'die lip + temperature control + haul-off': optical sheets need thickness closed-loop; use the thickness curve to locate the problematic die lip section for transverse deviation and adjust it targetedly.