ظاهرة المشكلة
Qualified PE parts warp and deform after packing and transportation, leading to customer complaints.
تحليل الأسباب
Products are packed before being fully cooled to room temperature; residual heat plus stacking load makes PE, which already has obvious creep, continue to slowly deform inside the package; an inner-liner design with locally concentrated stress also fixes the deformation into a specific shape, becoming a permanent defect by the time it reaches the customer.
الحل
①Fully cool products to room temperature before packaging; ②Optimize the packaging liner to distribute the load; ③Control the number of stacking layers and packing temperature; ④Design shape-setting liners for easily deformable parts; ⑤Evaluate the logistics environment temperature.
الخلاصة الأساسية
PE 'packing hot parts = secondary deformation': packing only after thorough cooling is the bottom line, and load distribution by the liner is the guarantee; PE creeps greatly, so the temperature and pressure in the logistics stage must both be taken into consideration.
PE;deformation;packaging;creep;stacking