Production & Quality 8 مشاهدة

Sink Marks on PEEK Orthopedic Implants

ظاهرة المشكلة
Surface sink marks on PEEK orthopedic implants are out of tolerance; dimensional accuracy and surface quality cannot meet medical standards, and simply adjusting holding pressure gives unstable results.
تحليل الأسباب
The uneven wall thickness and fine structure of the implant make feeding channels complex; PEEK crystallization shrinkage and the holding window are mutually coupled, and when the holding curve is unreasonable, local feeding is insufficient, forming sink marks.
الحل
①Optimize the injection and holding curves based on Moldflow simulation; ②Use staged holding to match the freezing sequence of each region; ③Control mold temperature in stages to balance crystallization shrinkage; ④Place the gate near the thick-wall functional area.
الخلاصة الأساسية
Sink mark treatment for PEEK medical parts requires simulation-driven holding curve design; staged mold temperature control is an effective means for precision medical parts; once the process is fixed, it must be strictly controlled.
PEEK;implant;sink mark;holding curve;medical;simulation