Material Drying
5 مشاهدة
PET regeneration drying management
ظاهرة المشكلة
After the dryer molecular sieve has been used for two years, the dew point cannot be raised
تحليل الأسباب
The adsorption capacity of the molecular sieve decays with use, and when regeneration is incomplete, the drying capacity is gradually lost; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
الحل
Establish a molecular sieve life ledger; force a regeneration check when the dew point exceeds -30℃; replace every 2-3 years; after adjustment, take consecutive samples to verify the effect, and resume mass production only after confirming stability
الخلاصة الأساسية
The molecular sieve is a consumable, and its life is managed by the dew point indicator; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems
هل كان هذا مفيدًا؟
0 شخص وجدوا هذا مفيدًا
شكرًا لك على ملاحظاتك!