PET oven handle
ظاهرة المشكلة
Oven PET handles deform and loosen at high temperatures
تحليل الأسباب
The oven door temperature can reach above 100℃; ordinary PET has insufficient heat distortion temperature; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
الحل
Select glass-fiber-reinforced heat-resistant grades for oven parts; or switch to PBT/bakelite; heat insulation design for metal inserts; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
الخلاصة الأساسية
Oven accessories must be selected with heat-resistant materials according to actual temperature rise; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
هل كان هذا مفيدًا؟
0 شخص وجدوا هذا مفيدًا
شكرًا لك على ملاحظاتك!