Processing Machinery 5 مشاهدة

PMMA Melt Temperature Range

ظاهرة المشكلة
PMMA melt temperature set at 260℃, products yellow and bubbles increase
تحليل الأسباب
Above 250℃ PMMA melt thermal degradation accelerates, and methyl methacrylate monomer is released forming bubbles and yellowing; During on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based on experience alone.
الحل
Melt temperature controlled at 200-250℃; optical parts take 220-240℃; overheated material must be purged and must not be used; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability.
الخلاصة الأساسية
PMMA melt upper limit is 250℃, and over-temperature degradation is irreversible; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence.; include this case in the defect archive as a troubleshooting reference for similar future problems.
PMMA melt temperature degradation bubbles