Injection Molding 6 مشاهدة

Ripples (flow marks) on PP products

ظاهرة المشكلة
Concentric circular ripples appear around the gate, or wavy patterns appear along the flow direction, obvious on high-gloss surfaces.
تحليل الأسباب
The melt front advance speed is unstable and the front temperature drops too fast, leaving ripples on the cavity surface; low mold temperature, an unreasonable injection speed curve, and a gate that is too small cause the front to 'stop and go' or cool locally.
الحل
①Optimize the injection speed curve to keep the front smooth; ②appropriately increase the mold temperature and melt temperature; ③enlarge the gate to reduce local throttling; ④check the temperature uniformity of the hot runner; ⑤adjust the gate position when necessary to improve the flow pattern.
الخلاصة الأساسية
PP ripples are the externalization of the front's 'disrupted rhythm': smooth the speed curve and preserve the front temperature, and the ripples will disappear; it is essentially a filling stability problem, not a surface treatment problem.
PP; ripples; flow marks; front; speed curve; mold temperature