Processing Machinery 5 مشاهدة

PPO Internal Voids

ظاهرة المشكلة
[Problem Phenomenon] Internal voids in thick-walled PPO products, detected by X-ray or sectioning
تحليل الأسباب
In thick-walled areas, the outside solidifies first and the internal shrinkage has no material to compensate, forming vacuum voids; insufficient holding compensation and excessive wall thickness act together; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
الحل
Uniform wall thickness design to reduce material; staged holding pressure to extend compensation; strengthen core cooling of thick-walled parts to guide directional solidification; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
الخلاصة الأساسية
PPO voids are a cut-off of compensation supply, and wall thickness uniformity comes before holding pressure adjustment; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future