PPS Flash and Overflow

ظاهرة المشكلة
Severe flash at the parting line and ejector pins of PPS products, requiring cleaning almost every shot.
تحليل الأسباب
PPS melt has excellent fluidity (low viscosity) and easily penetrates tiny mold gaps; insufficient parting line fit accuracy, insufficient clamping force or excessive injection pressure all form flash.
الحل
①Control parting line fit accuracy within 0.01mm; ②check and increase clamping force; ③reduce injection pressure and speed; ④repair worn parting lines and inserts.
الخلاصة الأساسية
Flash is the number one problem in PPS processing; its low-viscosity characteristic requires mold fit accuracy far higher than conventional engineering plastics.; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
PPS;flash;overflow;parting line;clamping force;accuracy